Nickel & Cobalt Based Superalloys
*All compositions represent the Nominal Composition in %
| Aimtek Alloy No. | Industry Specifications | Nominal Composition (Percent %) Ni (%) | Nominal Composition (Percent %) Co (%) | Nominal Composition (Percent %) Cr (%) | Nominal Composition (Percent %) Ti (%) | Nominal Composition (Percent %) W (%) | Nominal Composition (Percent %) Others (%) | Common Applications |
|---|---|---|---|---|---|---|---|---|
| T-400 | B50TF155 B50A918 EMS52432 Type XVI EMS56712 BMS10-67 Type XV CTS1025 | 60.4 | 8.5 | 28.5 Mo, 2.6 Si | Repair of Cobalt based superalloy casting components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; intermetallic Laves phases provide excellent wear properties to 1500°F (816°C); good hot hardness, oxidation, and corrosion properties; low coefficient of friction | |||
| T-800 | B50TF190, B50TF193 EMS52432 Type XV EMS56713 | 50.6 | 17.5 | 28.5 Mo, 3.4 Si | Repair of Cobalt based superalloy casting components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; intermetallic Laves phases provide excellent wear properties to 1500°F (816°C); good hot hardness, oxidation, and corrosion properties; low coefficient of friction | |||
| Mar-M-247 | PWA36117-2 EMS55447 EMS54752 Type XXIII BZ-003 Type 19 B-64 | 59.8 | 10 | 8.4 | 1.05 | 10 | 5.5 Al, 3.05 Ta, 1.4 Hf, 0.65 Mo, 0.15 C, 0.015 B, 0.05 Zr | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys |
| IN713C | PWA36118-1 AMS5391 (chemistry only) | 71.64 | 14 | 1 | 6 Al, 4.5 Mo, 2 Nb+Ta, 0.85 Zr, 0.01 B | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; wide gaps and wear resistant coatings | ||
| L-605 | B50A919 | 10 | 53.5 | 20 | 15 | 1.5 Mn | Excellent high temperature strength and good oxidation resistance; service temperatures up to 1795°F (980°C) | |
| X-40/Alloy 31 | PWA1316 PWA1318 MSRR9507/3 MSRR9500/23 CPW218 CPW236 B50TF185 EMS52432 Type XXIII AMS5791 BMS10-67 Type IX DMR33.007 DMR33.008 DMR33.351 CL. 2 MS1087 | 10.5 | 56 | 25.5 | 7.5 | 0.5 C | Replaces Tungsten Carbide in high temperature applications; excellent oxidation resistance; repair of Cobalt based superalloy components made from same alloy; crack repair and restoration when mixed with activated diffusion braze alloys | |
| CM-64 | PWA1314 PWA694 B50A842 B50TF55 MSRR9500/226 DMR34.070 MTS1087-1 | 5 | 45.15 | 28 | 19.5 | 1 V, 0.85 C, 0.5 B | Excellent high temperature wear and oxidation resistance; repair of Cobalt based superalloy casting components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; service temperatures up to 1350°F (732°C); hard, dense coatings | |
| Merl 72 | PWA795 MSRR9500/248 B-72 | 15 | 46.85 | 20 | 0.2 | 9 | 4.4 Al, 3 Ta, 1.15 Hf, 0.35 C, 0.04 Y | Excellent high temperature wear and oxidation resistance; repair of Cobalt based superalloy casting components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; hard, dense coatings |
| FSX-414 | B50A489 | 10.5 | 52.2 | 29.5 | 7 | 0.8 Si | Good oxidation resistance; repair of Cobalt based superalloy casting components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys | |
| Alloy 6 | B50A960 MSRR9500/19 | 66 | 28 | 4 | 1 Si, 1 C | Excellent high temperature wear and oxidation resistance; repair of Cobalt based superalloy casting components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; hard, dense coatings | ||
| H188 | B50TF255 B-17 | 22 | 41.15 | 22 | 14.5 | 0.35 Si | Repair of Cobalt based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys | |
| Mar-M-509 | PWA1185-2 B50A988 B50TF304 CPW549-2 MS1068 B-60 | 10 | 54.75 | 23.5 | 0.25 | 7 | 3.5 Ta, 0.6 C, 0.45 Zr | Repair of Cobalt based superalloy casting components made from same alloy, such as airfoils, combustors, blades, vanes; crack repair and restoration when used with activated diffusion braze alloys |
| IN625 | MTS1438 ST1627 | 63.3 | 21.5 | 9 Mo, 3.7 Nb+Ta | Excellent high temperature oxidation and corrosion properties; repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; service temperatures up to 1800°F (982°C) | |||
| IN718 | B50TF202 MS1088 AMS5832 (chemistry only) | 53.9 | 19 | 1 | 18 Fe, 5.1 Nb+Ta, 3 Mo, 0.5 Al | Excellent high temperature oxidation and corrosion properties; repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; service temperatures up to 1800°F (982°C) | ||
| IN738 | 60.84 | 8.5 | 16 | 3.4 | 2.6 | 3.4 Al, 1.75 Mo, 1.75 Ta, 0.9 Nb, 0.11 C, 0.05 Zr, 0.01 B | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys | |
| IN939 | 48.25 | 19 | 22.5 | 3.7 | 2 | 1.9 Al, 1.4 Ta, 1 Nb, 0.15 C, 0.1 Zr, 0.01 B | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys | |
| Rene 142 | MODS210289 | 58 | 11.7 | 6.8 | 4.9 | 6.35 Ta, 6.1 Al, 2.8 Re, 1.5 Mo, 1.5 Hf, 0.12 C, 0.015 B | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys | |
| Rene 77 | 58.45 | 15 | 14.6 | 3.35 | 4.3 Al, 4.2 Mo, 0.07 C, 0.016 B | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys | ||
| Rene 80 | B50TF183 MS1086 MS1158 CD1146 C-74 | 60.5 | 9.5 | 14 | 5 | 4 | 4 Mo, 3 Al | Repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys; wide gaps and wear resistant coatings |
| C276 | 58.2 | 15.8 | 4 | 16.5 Mo, 5.5 Fe | Excellent high temperature oxidation and corrosion properties; repair of Nickel based superalloy components made from same alloy; crack repair and restoration when used with activated diffusion braze alloys |